MG+ Membrane Press Adhesive
PROPERTIES
Type : Waterborne Synthetic Emulsion ( PU based )
Colour: Milky White
Viscosity : 450-700 cPs
Solid Content : 60% ( +/- 2% )
pH: 4-7
Sealing Temperature : 70-80°C
Drying Time: Approx 5-15 minutes depending on temperature, Humidity and applied quantity
Hardener Mixing Ratio : We recommend adding 5% HARDENER “WB-MPA” for heat / thermal resistance.
(Hardener is added to applications which come in direct contact with heat / sunlight )
Packaging Available : 20kg plastic bucket with spout ( for easy usage )
MG+ Membrane Press Adhesive
Request a Call Back
- Ask a Question
MG+ Membrane Press Adhesive
Ask a Question
- Brushale Synthetic Ruber Adhesives (SR Adhesives) 14
- Sprayable Synthetic Rubber Adhesives (Spray Adhesive) 4
- Toulene Free Rubber Adhesives (TF) 4
- Natural Rubber Adhesives (NR) 2
- Membrane Press Adhesives (3d Lamination Glue) 6
- Footwear Bonding Pu Adhesives 6
- Primers For Footwear 4
- Cleaners For Footwear 3
- Hardeners For Footwear 2
Related Products
Applications :-
PVC laminated wooden doors.
Advantages :-
Good coverage.
Long lasting bonds and water resistant properties (after mixing of Hardener CB).
Ease of application.
Mild smell.
No harmful benzene
PROPERTIES
Type : Waterborne Synthetic Emulsion
Colour: Milky White
Viscosity : 200-450 cPs
Solid Content : 55% ( +/- 2% )
pH Scale: 4-7
Sealing Temperature : 60-70°C
PROPERTIES
Type : Waterborne Synthetic Emulsion
Colour: Milky White
Viscosity : 250-600 cPs
Solid Content : 55% ( +/- 2% )
pH Scale: 4-7
Sealing Temperature : 60-70°C
Drying Time: Approx 5-15 minutes depending on temperature, Humidity and applied quantity.
Hardener Mixing Ratio : We recommend adding 5% HARDENER “WB-MPA” for heat / thermal resistance.
(Hardener is added to applications which come in direct contact with heat / sunlight )
Packaging Available : 20kg plastic bucket with spout ( for easy usage )
DESCRIPTION :
HARDENER “ WB-MPA”
“WB-MPA” is a cross linkingagent that Is used for increasing the heat resistance & water resistance of the bonded / laminated PVC foil.
We recommend adding 5% of the cross linker with the main adhesive for better and improved performance.
TYPE : Isocyanide hardener
COLOUR : Transparent
HARDENER MIXING RATIO : We recommend adding 5% HARDENER “WB-MPA” for heat / thermal resistance.
(Hardener is added to applications which come in direct contact with heat / sunlight )
PACKAGING AVAILABLE : 1kg metal bottle
PROPERTIES
Type : Waterborne Synthetic Emulsion ( PU based )
Colour: Milky White
Viscosity : 300-650 cPs
Solid Content : 55% ( +/- 2% )
pH: 4-7
Sealing Temperature : 60-70°C
Drying Time: Approx 5-15 minutes depending on temperature, Humidity and applied quantity
Hardener Mixing Ratio : We recommend adding 5% HARDENER “WB-MPA” for heat / thermal resistance.
(Hardener is added to applications which come in direct contact with heat / sunlight )
Packaging Available : 20kg plastic bucket with spout ( for easy usage )